2018022:3月19日至3月26日亚太区域典型缺陷

13月19日至3月26日典型缺陷1

中国检查艘次滞留船舶艘次滞留率15785.09%典型缺陷举例缺陷代码05105     MF/HF Radio installation缺陷描述MF/HF radio installation (primary systems specified in S.R cert)found malfunction (30)缺陷照片

2澳大利亚检查艘次滞留船舶艘次滞留率6934.34%典型缺陷举例缺陷代码02116      Bulkheads - cracking缺陷描述Cracks found on six out of eight temporary welds on side bulkhead (F48P, F69P& S, F95P& S, F121P) between decks 4 and deck 5. Welding carried out by ships crew. Cracks length range from 300mm-600mm long .      crew. Cracks length range from 300mm-600mm long.Load Lines, S74/CI/PB/R11 (30)缺陷照片

3日本检查艘次滞留船舶艘次滞留率6011.66%典型缺陷举例缺陷代码03105     Covers (hatchway-, portable-, tarpaulins, etc.)缺陷描述Bulkhead between other machinery spaces(air conditioning machinery)and corridor-not indicated a-0 class (30)。缺陷照片

4俄罗斯检查船舶艘次滞留船舶艘次滞留率29413.78%典型缺陷举例缺陷代码18417     Anchoring devices缺陷描述Port side anchor and chain -missing( was lost at KWANGYANG, S. KOREA anchoring) (99)缺陷照片

编者注:典型缺陷均由编者从APCIS数据库选取,仅供PSC相关人员学习参考,不代表东京备忘录秘书处及本平台观点。